Jun 13, 2007 #1 kevlar49 Materials Joined Jun 1, 2006 Messages 287 Location US Does anyone know of any problems with using Nitronic 50 stems in boiler feed water valves operating around 200°F?
Does anyone know of any problems with using Nitronic 50 stems in boiler feed water valves operating around 200°F?
Jun 13, 2007 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US I don't see any problem with using N50 at your conditions. I would use the 1950F annealed material. I've used N50 and N60 all around boiler feed water pumps and valves. Upvote 0 Downvote