Nitronic 60 vs nitrided (liquid) 17/4 drum and sleeve on split case pumps.
Nitronic 60 on numerous parts on all SS centrifuges where incidental contact is possible.
Nitronic 50 on shafts for the above centrifuges.
Nitronic 50 for vertical multistage pump shafts, especially where operation is intermittent.
Nitronic 60 for spinnerettes replacing 316 SS.
Nitronic 60 for wire inserts, Helicoils.
Nitronic 60 for threaded parts especially nuts for set in studs.
Nitronic 50 for large boat shafts.