Feb 16, 2016 #1 metalonis Mechanical Joined Feb 28, 2002 Messages 183 Location US Is there an ASM (or other) specification for a suitable process for nitriding screw threads in annealed austenitic stainless steel?
Is there an ASM (or other) specification for a suitable process for nitriding screw threads in annealed austenitic stainless steel?
Feb 16, 2016 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US I do not know of any consensus standards, but here are two processes used in industry for threaded parts: http://www.nitrex.com/technologies/#nitregs http://www.expanite.com/ Upvote 0 Downvote
I do not know of any consensus standards, but here are two processes used in industry for threaded parts: http://www.nitrex.com/technologies/#nitregs http://www.expanite.com/
Feb 16, 2016 Thread starter #3 metalonis Mechanical Joined Feb 28, 2002 Messages 183 Location US Thanks CoryPad. BTW, I meant AMS, not ASM. Upvote 0 Downvote
Feb 16, 2016 #4 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US You can try SAE AMS2759/6B Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts and SAE AMS2759/10A Automated Gaseous Nitriding Controlled by Nitriding Potential. Upvote 0 Downvote
You can try SAE AMS2759/6B Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts and SAE AMS2759/10A Automated Gaseous Nitriding Controlled by Nitriding Potential.