Is there an ASM (or other) specification for a suitable process for nitriding screw threads in annealed austenitic stainless steel?
 
Thanks CoryPad. BTW, I meant AMS, not ASM.
 
You can try SAE AMS2759/6B Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts and SAE AMS2759/10A Automated Gaseous Nitriding Controlled by Nitriding Potential.
 