Im after some specs on nitrided H13 tool steel, namely die Ejector pins. My supplier cant help, and matweb hasnt been much use.

Would like to know approx depth and hardness of the nitrided layer, tensile strength core hardness etc.

Im mainly using 3/16, 1/4 and 7mm Dia.


Was told it couldnt be done, so
i went and did it!
 