I am nitriding a threaded shaft of 4140 (approx 2" OD). I am looking for a case hardness of at least 50HRc after a nitriding treatment at 1075F for 90 minutes (repeated once). I want a case depth of 0.002" and a return to HRC 33 max at a depth of 0.006". I have not had lkuck attaining these results, any suggestions?
Also, utilising the same procedure for 17-4 is not producing the desired results either. I am not that familiar with nitriding. I am wondering if anyone has any suggestions? I am trying to achieve the same results as was described for 4140. Thus far, I am achieving around 40HRc for the 17-4. Is the time or temperature for nitriding insufficient? Or, is the expectation of 50HRc unreasonable?
Also, utilising the same procedure for 17-4 is not producing the desired results either. I am not that familiar with nitriding. I am wondering if anyone has any suggestions? I am trying to achieve the same results as was described for 4140. Thus far, I am achieving around 40HRc for the 17-4. Is the time or temperature for nitriding insufficient? Or, is the expectation of 50HRc unreasonable?