Hi,
I am trying to reduce my nitrate levels so that we are below our license limit. The main contributor to the nitrate level is a pickling solution which contains 35% nitric acid, 1.5% hydrogen peroxide and up to 1% nickel. Only 200 litres are dumped every 48 hours. We can reduce the nitrates to nitrites as our allowable limit for nitrites is much higher but biological treatment is not feasible for such a small volume. Please advise!
Thanks,
Chemicalenvironment
I am trying to reduce my nitrate levels so that we are below our license limit. The main contributor to the nitrate level is a pickling solution which contains 35% nitric acid, 1.5% hydrogen peroxide and up to 1% nickel. Only 200 litres are dumped every 48 hours. We can reduce the nitrates to nitrites as our allowable limit for nitrites is much higher but biological treatment is not feasible for such a small volume. Please advise!
Thanks,
Chemicalenvironment