I'm not quite sure what you are calling a nipplet? Theres sockolets,threadolets and weldolets. But if you drill the hole in the blind flange where the 1/2" nipple were to pass completely through and then weld a filet weld around the nipple on the inside and the same on the outside you should then not have any trouble or worries of failure.