Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Nipoflanges, Flange olets, Long Weld Neck Flanges

Status
Not open for further replies.

ryanvg42

Mechanical
Joined
Feb 19, 2014
Messages
1
A question has been raised if the below picture is considered a nipoflange or flange olet? It appears to be on long weld neck flange that has been beveled and installed on on 20" main header.
1. Is this a nipflange or flange olet
2. Besides the incompleted weld would this be exceptable per B31.3
A. If not acceptable why? The thickness of the pipe is the entire thickness of a weldolet and would appear to be stronger.
3. It could possibly be a bad manufacture that is calling it a nipoflange per the MTR, in which it is a long weld neck flange.

ANy feedback we would great.
 
 http://files.engineering.com/getfile.aspx?folder=caa12a1a-7efe-4eae-bede-489e2eedc97c&file=IMG_4055.JPG
Looks like a nipolfange, 300#, Sch 160 body or Sch 40, hard to see. A Long Weld Neck would not have any Schedule. Acceptable in B31.3 within the Temp/Pressure Ratings for 300# SA-350-LF2 CL.1
 
Its hard to determine if all of this is correct.

First, the type of fitting needs to be known I think. Then, using the rules from para 304 in B31.3 for branches, you can determine if this weld is acceptable (one option is this is an intergally reinforced fitting (like per MSS SP-97), which could waive calcs for reinforcement zone). Keep in mind that the design conditions may play a role here to determine if the weld is acceptable (it may e.g. need a fillet).

Without knowing all this, I would suspect this weld is unacceptable.

And why is corner profile welded to it? This would make a nice tress riser
 