Hi,
Does Nickel silver material suite as a cover for electronic elements?

Thanks, Aharon
 
Replies continue below

Recommended for you

Can you possibly elaborate a little more? What kind of cover are you talking about? Why do youn not want to use aluminum?

TTFN
 
TTFN,
The cover actually use as an isolator box for photo receiver element.
I can’t use aluminum because cover thickness is 0.1 mm.
Aharon
 
Why are you forcing the cover to be so thin? It will hardly provide structural protection.