All,

I am a newbie at doing PV design, and i have been given a job to quote. They are calling out
SA-516-70 1.188" Nom Clad with SB-162-200 .281" nom for the shell material and similar for the head.

They are using these specs off an existing tank that has been working flawless. Does anyone know of a vendor that can make such a material? I have been coming up empty handed.

Thanks in advance
 
Replies continue below

Recommended for you

BDaugherty, for roll clad, Mittal Steel

For explosion bond, Dynamic Metals

You'll find them on the web.