Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Ni-Cd Battery sizing by Hoppecke Power-Line-Designer Software

Status
Not open for further replies.

AbbasAF

Electrical
Joined
Apr 29, 2007
Messages
1
Location
IR
I have access to Hoppecke software "power-line-designer" but unfortunately I can't register for use of it.
could anyone possibly do the battery sizing calculation for the below case and inform me about the result / report.
Battery Type: Ni-Cd M-Type (HOPPECKE FNC-M)
Number of Cells: 90
Load Type: UPS
Load Period 1: 3910W, Duration (H:M:S): 00:30:00
Load Period 2: 1624W, Duration (H:M:S): 01:30:00
Total Duty Cycle (H:M:S): 02:00:00
Aging Factor: 1.10, Design Margin: 1.10
Nominal. Temp.: 25C, Lowest Temp.: 0C, Highest Temp.: 40C
Max. System Voltage: 135V, Min. System Voltage: 102.6V,Charging Voltage per Cell: 1.5V, End Voltage per Cell: 1.14V, Nominal System Voltage: 108V