We could not find any reference to grooved joints in piping in NFPA 14.

¿Are they allowed as a piping joining method in non sprinkler protected spaces?
 
Replies continue below

Recommended for you

NFPA 14-2013 4.4.3 Groove Joining Methods

4.4.3.1 Pipes joined by grooved fittings shall be joined by a listed combination of fittings, gaskets and grooves.

Good to go.

R M Arsenault Engineering Inc.
 
skdesigner:

Thanks for the information.

NFPA 14 requires protection of piping in enclosing with same fire rating as stairway enclosure.
 