Dear All,

I want to make a new WPS for past PQR. is there any limitation about thickness of basemeta?the process welding is GTAW and SMAW

Thanks in advance
 
Replies continue below

Recommended for you

Yes. Follow the requirements in Articles II and IV in Section IX using the PQR data.
 
You can make a new WPS from an existing PQR. The limits on thickness in the new WPS are essential variables based on the original PQR. Please review ASME IX, QW-403.8, QW-451 & QW-202.4(b) (if applicable).

 