Dear Expert.
I have Material SA 517 gr B
I want to prepare PQR,with process SMAW (Root+Filling) and Capping of SAW.
please suggest Electrode for SMAW and Filler wire and flux for SAW
 
Do you have a copy of ASME Section II, Part A; SA 517 Gr B? Do you know the minimum YS and TS requirements for this Grade?

Do you have a copy of ASME Section II, Part C? Filler metal specifications?

If you do, review SFA 5.5, Table 3

For SAW review SFA 5.23, Table 1 and Table 8

 
i reviewed and select E 12018. is it right?
 
From my experience, E12018 is typically used with SA-517 Grade B material. This is a P11B material and usually requires impact testing and post weld heat treatment. Especially if used on a DOT pressure vessel.
 
And what about 517 Gr A thickness 8 mm? it require PWHT or not?
 
What is your design Code? Is this a DOT vessel?
 