Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

New concrete slab on top of existing

Status
Not open for further replies.

greznik91

Structural
Joined
Feb 14, 2017
Messages
186
Location
SI
Im dealing with insufficient existing RC slab above a residental building (first floor). Existing slab is aprox. 120 mm thick but reinforcement is unknown. the problem is that a slab cant be removed (and replaced with new one).

The slab is vibrating if you jump. There was a screed (100 mm) above this slab that is now removed.

I was thinking about making a new RC slab above existing (spans are small) so I was thinking about making it 100 - 120 mm thick. I would design a new slab so it would be sufficient alone (im not considering existing slab below). There would be no connection (no anchors for a horizontal shear between existing and a new slab). I know it would be easier to just remove existing slab and make a new one but thats not a possibility.

my question is how much load is to be expected on existing slab bellow since a new one is made on top of it?
Do loads distribute based on stiffness since there is no horizontal connection between both slabs?
In worst case scenario, the load of a new slab is approx. the same as 100 mm of screed that has been removed.

When pouring a new slab the existing slab would be used as a formwork (wtih some supports bellow it) - as I said spans are small.

Your thoughts?

apologies for my poor english


QA_ly4glh.png
 
Id really appreciate some thoughts about this.
 
I would want to make the slabs work compositely. This can be done merely by ensuring the existing slab is thoroughly clean and slightly roughened by shotblasting.
 
Is this an elevated slab?

Have you explored FRP strengthening?
 
If you pour a new slab on top of the existing, make sure that the foundations are adequate to support the additional load; also, you might want to add a few temporary shores under the existing slab until the new concrete has cured.

The existing slab and the proposed slab both seem rather shallow for the 5 m span, so composite behavior as suggested by hokie66 might be a prudent plan.

BA
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top