Neoprene O-ring gasket

Status
Not open for further replies.

engpes

Mechanical
Feb 10, 2010
175
I am trying to determine the gasket factor, m, and the seating stress,y, of a 1/2" neoprene type o-ring gasket.

ASME VIII, Div 1 (table 2.5-1) states that these are self-energizing and that the m and y values are both zero.

Can I really use valued of 0 for both of these? I am trying to determine my bolt loads required to seal.

Thanks in advance.
 
Replies continue below

Recommended for you

Parker manual on line

depending on whether static or dynamic seal, the goal is initially to compress the o-ring 10% or so, and that is built into the geometry via groove dimensions.
If the bolts are securing a cover, then they must apply enough preload to clamp metal-to-metal (easy) and also withstand whatever maximum pressure is going to be without allowing the joint faces to separate and release or even just upset the o-ring.

Improper finishes on any of the 3 sealing surfaces can create a curious problem situation with leaks at low pressure, OR high pressure OR when pressure changes.
 
engpes, confirm, m & y = zero for O-ring gasket.

Please note, you are not determining bolt loads required to "seal", just bolt loads to use for flange design.

Regards,

Mike
 