Hello,
I am studying a case in which static waterproofness is done using neoprene seals.
The one is of EE-31B6, the other is of EE-20A8.
To evaluate the stress these seals are submitted to under initial mounting I am seeking for informations about :
compression load at 5% to 50% (if available),
permanent stress.

Thank you.

 