Hello,

I'm looking for a suggestion to fix a component with a weight: Upto 2000 KG rigidly in a compartment. I have attached a step file of an assembly. The red part was the component that I'm trying to fix. Initially, we tried one concept(attached image) but it didn't work the bolts were sheared off.

We have only 4 wedges on the Red part. Is there any better mechanism to lock that Red Part rigidly? Your suggestions are greatly helpful.

Thank You..!


Thanks & Regards,
Sam
 
 https://files.engineering.com/getfile.aspx?folder=04982522-e66a-42df-b0bd-3249c2b1131a&file=Componnet.zip
Replies continue below

Recommended for you

Hi shanmuk44

I can’t open a step file, can you make it a pdf or some png format or just paste some photos of the component.

“Do not worry about your problems with mathematics, I assure you mine are far greater.” Albert Einstein
 
How much vibration and shock load is there on this?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
We are doing 5G FEA on those components but the bolts were sheared. Then we tried for use wedge jack mechanism but they were no enough space.

Thanks & Regards,
Sam
 