I need a cylinder/tube/pipe made of GE Plastics Valox. Specifically, 420HP, 7062 HP and IQ3001, though preliminary tests can be made using anything in the Valox family.

Any other suggestions for posting?

Truly appreciate you guys and this website!
 
Replies continue below

Recommended for you

Make a drawing and put it out for quote, e.g. on mfgquote.com.



Mike Halloran
Pembroke Pines, FL, USA
 


Hmmm.. Valox 420HP is a 30% Glass reinforced PBT - injection moulding grade.

You will be lucky to find barstock in this (or any other PBT) to make a sample of. Try searching for other makes of PBT in barstock - cannot find one in UK.

Otherwise a prototype alloy tool and to mould it is the solution.


Cheers (and Good Luck)


Harry
 