In rolling and reeling flat wire, we use finger-type guides for the wire wrap. What steel would be good to use, that would be "springy" enough to hit the sides of the reel without breaking or bending? I had thought the guide that is already on the line was stainless, but it has some very strong magnetic characteristics. The guide would be on the order of 2mm by 40mm and is approximately 11 inches long.
Any suggestions would be welcome. Thanx!