Let me start off by saying I’m not a metallurgist, I’m a chemical engineer. I have a metallurgist problem though! I bought a stainless steel stock pot, which has some small rust spots/streaks on the bottom after an hours-long soak in tap water. I understand I need to re-passivate it. The manufacturer of the pot told me it’s 18/0 steel, which I think means it’s the same as 430. I have the chemicals (nitric acid and NaOH) needed to passivate it, but I don’t know if its 430 or 430F/FR. There are different passivation methods for the two, correct?
How can I tell? Will it hurt to be safe and follow the NaOH regimen with 430, even though it doesn’t need it?
Thanks in advance for your help!
How can I tell? Will it hurt to be safe and follow the NaOH regimen with 430, even though it doesn’t need it?