need to install concrete in water to fortify undermined footer

Status
Not open for further replies.

guy333

Materials
Joined
Aug 8, 2009
Messages
1
Location
US
any advise on this ?

 
Humm.. Page cannot be found. Need a few details, and I can help. I've spent 40 years doing underwater and waterfront engineering projects, including foundation shoring under water. If you can't build a form, stack bags of pre-mixed concrete in place, assuming you have a foundation on which they will stay. The bag lasts long enough to set the concrete. However, the devil is in the details. I'd need to see the details to really be able to help.

 
Not a difficult thing to do .Use fabric formwork bags and just pump from above down an appropriate line.As above the ramifications are in the details. You may need to grout any voids behind the bags.

Intrusion Prepakt /marineconcrete.com
 