I have a list of components in some metal samples found in my product by customers.

It is 88.2% Fe with the following additives:
8200 ppm Mn
1000 ppm Cr
2900 ppm Ca
1800 ppm Al
1500 ppm Co
857 ppm Ni

With traces of Mg, K, Co, and several others.

Is there a website that would list what grade of stainless this is? Thanks for replys
 
Are you sure of the chemical analysis?
1000 ppm Cr = 0.1% Cr and
857 ppm Ni = 0.0857% Ni would not make up a stainless.
It is not clear why your customers should find the composition of your products.

 
I didn't do the analysis, so I have to go by what the numbers say.

I dug a little further and found out some more info.

My product is food grade powdered sugar. Our customer runs the product across magnets as it unloads from a rail car. They found 'highly magnetic' pieces on the magnet after processing a certain car that had my product in it. The samples were sent to my home office and analyzed with the above results.

Thinking about it a little more, I realize this is not stainless (especially with the low chromium and nickel numbers). I asked for carbon content, but the sample was consumed in the first test and carbon was not analyzed.

I'm sorry if this is in the wrong forum. I didn't see a steel group. Mods can move as necessary.
 
Nah, it wasn't welding slag.

Current thinking is a bearing came apart somewhere in the process and the magnets and metal detector didn't catch it.
 