Hi everybody,

Has anybody heard of "peralumen"? not sure of the spelling, I think it might be an aluminium alloy, what I am looking for is details strength and properties of the material.

Does anybody out there know about it or know where I can find information about it?

Thank you very much in advance for your help.

gg
 
Replies continue below

Recommended for you

I'm not familiar with the details, but I've seen several references to "Peralumin". A Google on that may help

Good Luck
johnwm
 
Hi,

PERALUMAN (not peralumEn and not peralumIn) is an aluminum alloy. There are different grades of peraluman such as Peraluman - 300 (AlMg3), Peraluman - 460 (AlMg4.5) and so on. You can go on the following website to find info on Peraluman - 300, and if you do a search on you'll find more info.


Good luck

Coka
 
Thank you both very much found what I needed.

Always grateful for sites like this and people like you.