Hello
I just came across this site, which looks like a wealth of useful information.
I have a project where I have been tasked to try some different surface treatments on AL6X.
My test plan requires that I first get the material to pit. This is proving extremely difficult.
If anyone knows any recipe/testing methodology for getting this material to pit, it would be greatly appreciated.
thanks
I just came across this site, which looks like a wealth of useful information.
I have a project where I have been tasked to try some different surface treatments on AL6X.
My test plan requires that I first get the material to pit. This is proving extremely difficult.
If anyone knows any recipe/testing methodology for getting this material to pit, it would be greatly appreciated.
thanks