Jan 15, 2004 #1 410 Industrial Joined Jan 15, 2004 Messages 1 Location US These materials were spec'd for building the Browning 1919A4 machine gun. Mil-spec was QQ-S-624. Any leads on where to find info on this mil-spec also appreciated.
These materials were spec'd for building the Browning 1919A4 machine gun. Mil-spec was QQ-S-624. Any leads on where to find info on this mil-spec also appreciated.
Jan 15, 2004 #2 NickE Materials Joined Jan 14, 2003 Messages 1,570 Location US You can find the chemistry and physical properties on: http://www.matweb.com you will likely find that several of the materials are no longer used. I'm not sure where to find old military materials spec. you might try a military history group or an office like that in the defense dept. nick Upvote 0 Downvote
You can find the chemistry and physical properties on: http://www.matweb.com you will likely find that several of the materials are no longer used. I'm not sure where to find old military materials spec. you might try a military history group or an office like that in the defense dept. nick
Jan 15, 2004 #3 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US You can obtain the specification from ASSIST: http://assist.daps.dla.mil/quicksearch/ Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
You can obtain the specification from ASSIST: http://assist.daps.dla.mil/quicksearch/ Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.