I am looking for a casting epoxy that has good mechanical strength and high tempererature capability with a low CTE. We've tested BisA with 20% glass microbubble fill and have measured 25 uin/in-degF. We measured unfilled to be 35 uin/in-degF. I need an epoxy with a CTE around 13 uin/in-degF .
Please make recommendations on what else I can do to reduce the CTE? Different fillers? Different resin?
Thanks
Please make recommendations on what else I can do to reduce the CTE? Different fillers? Different resin?