I am looking to have a custom-made O-ring produced with tight tolerances. The required cross-section diameter is 0.139" ± 0.004". can you see the attached drawing and advise on the most cost-effective manufacturing method for this O-ring.custom o-ring.jpg
 
You are looking for a custom formed gasket? Also, there is no way those tolerances can happen with an elastomer. At best an all-around profile tolerance in the restrained condition.

In a similar application I used a vertical slot and rectangular gasket material such that more than half the width of the gasket was in the groove. In hindsight I would have put a matching groove on the other part. This allows controlled compression of the gasket and retains the gasket during assembly. With the circular profile, especially if it isn't custom molded, the gasket will continuously fight to leave the groove during assembly as even the slightest twist will be enough to not lie flat.

With rectangular material it's just a matter of cutting to length and gluing the ends. For a better seal use a scarf joint.

Other than that there are a number of custom gasket molding companies who can make the part you have above and you can apply those tolerances to the mold.
 
You are possibly over specifying on your design. An o-ring or any flexible seal is by definition: flexible - the actual final shape is going to vary unless measured in a constrained condition. Specifying +.001/-.000 on size dims is unrealistic for most fabrication processes for a flexible/elastomeric seal. Your specification as shown is more for the fabrication mold than the final part. If you are planning on using a face seal groove then you don't necessarily need a preformed seal, measure the interior path length of the seal groove and choose an o-ring with an equivalent inside circumference +/- . Your corner radii are gentle enough to lay the o-ring in the groove and it will follow. Sorry if I am describing something you already know but your question kind of leaves that undefined. Any major seal manufacturer can work with you on your design. Look up Apple Rubber, Parker, Pacific Seal, etc.
 
Last edited:
Having used a regular circular ring in a rectangular groove I can tell from experience that it absolutely will not stay. It will resist the bend in the corners with enough force to climb the groove wall and escape unless the groove is undercut to capture it, making a good estimate of compression more difficult. It ended with having to glue the ring in place, defeating the value of the extra volume in the groove. It wasn't too big a deal as it was to discourage water entry, but it was a hassle.
 
Custom O-rings are commonly made from rolls of O-ring stock. The groove should be slightly narrower than the O-ring cross-section to keep the O-ring in the groove. The stock should be cut slightly longer than needed so that the splice is under compression. Then you do not even need to glue the splice to get a perfect seal. O-ring seals are self-energizing and quite robust, which is why they are so commonly used.
 
I commonly use o-rings in regular (non-undercut) grooves without issues of ride-out/lift-up as long as the corner radii are not extremely tight.

20250702_112610.jpg
 
3DDave and  Compositepro, your guidance on o-ring cord stock is correct since the OP's seal is not close to a standard AS568 size. An option would be to redesign the seal parameters to be nearer to a -268 or -269 to allow use of an off-the-shelf part.
 
I commonly use o-rings in regular (non-undercut) grooves without issues of ride-out/lift-up as long as the corner radii are not extremely tight.

View attachment 14765
That looks like glue is being used at several places to retain that seal and note that the seal is out of the groove on the right side.
 
The groove needs to have clearance to the o-ring or the o-ring will rupture when compressed.

A dovetailed o-ring groove will allow the use of a round o-ring without glue.


The challenge is not stretching the o-ring as it's pushed through the dovetail opening.

Association for Rubber Products Manufacturers has tolerance classes. Class E1 is high precision and gives a diameter of 0.139 ±0.007".

A Buna o-ring is not going to maintain its original cross section for very long.
 
Last edited:
No glue used - the schmutz is just debris on a part returned from service. The part of the seal on the right is just I was lazy and did not push that area of the seal down and took a bad photo. :-) I place o‐rings in uncircular grooves without issue. No ruptures or squirms. Certainly, this is possible because of the use case of the equipment I design. 3DDave and Tugboat, the design details you point out are valid for the many uses and environments. The OP has not specified any operational parameters, so all options are open.
 
Last edited:
It does raise the question about using a soft wire core in extruded o-ring stock to enable the pre-forming of the stock for complicated routes.
 