i am facing a critical problem with one of my company pressure vessels used in transporting (propane and butane ) according to ASME 8
Here is the case :
while trying to weld a crack appears at front head at the semi trailers made of (ASTM A 517 grade B )
The crack was about L1 = 14 CM (crack no.1) as shown in fig and it passes through weld line between head and shell (12 mm ) we stop the crack and weld it using filler metal 11018 M notice that the thickness at front head range from (5.6 mm to 7.5mm ) .
The day after while we inspecting crack and ready to perform post weld heat treatment another crack appears of length L2 = 7cm (crack no.2) at distance around D1= 9 cm from first crack almost parallel to first crack .
While trying to preform same operation another crack appear (crack No.3) with length of L3=7 cm at distance around D2=10cm from crack no.2
i am facing a critical problem with one of my company pressure vessels used in transporting (propane and butane ) according to ASME 8
Here is the case :
while trying to weld a crack appears at front head at the semi trailers made of (ASTM A 517 grade B )
The crack was about L1 = 14 CM (crack no.1) as shown in fig and it passes through weld line between head and shell (12 mm ) we stop the crack and weld it using filler metal 11018 M notice that the thickness at front head range from (5.6 mm to 7.5mm ) .
The day after while we inspecting crack and ready to perform post weld heat treatment another crack appears of length L2 = 7cm (crack no.2) at distance around D1= 9 cm from first crack almost parallel to first crack .
While trying to preform same operation another crack appear (crack No.3) with length of L3=7 cm at distance around D2=10cm from crack no.2