Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

need answer to a API 653 9.6.4 question

Status
Not open for further replies.

mulp

Structural
Jan 14, 2011
1
There is a API605 tank that has corrosion in the welds. the welds have be excavated and repaired per API653. In API 653 9.6.1 thru 9.6.4 states that this a noncomformance or a weld flaw. when I look at SEC.12.1.3.2 states the welds need RT or UT over their full length. Am I looking at the correct sections if not what would be the correct sections.
 