I am modelling a necking problem.I want to get the engineering stress-strain curve. My specimen is 20mm length and 5 mm radious. I model the quarter section considering the axissymmetry and symmetry about horontal axis. My abaqus model 20 mm length and 5mm width. I use axisymmetry element CAX4. I applied uniform displacement load. I get my reactions along the node where i apply uniform displacement load. then, I add all the reaction, then divide by the 5mm (assuming the thickness of the model is 1 unit).
I see the necking. but my Stress-strain result seems to be NOT correct.
Plaese anyone advise me about my procedures are correct?
Thanks
Usitha
I am modelling a necking problem.I want to get the engineering stress-strain curve. My specimen is 20mm length and 5 mm radious. I model the quarter section considering the axissymmetry and symmetry about horontal axis. My abaqus model 20 mm length and 5mm width. I use axisymmetry element CAX4. I applied uniform displacement load. I get my reactions along the node where i apply uniform displacement load. then, I add all the reaction, then divide by the 5mm (assuming the thickness of the model is 1 unit).
I see the necking. but my Stress-strain result seems to be NOT correct.
Plaese anyone advise me about my procedures are correct?
Thanks
Usitha