Hey Guys,
when I have design temperature about 300 C grade for vessel pressure then
I have to use weld neck flanges for nozzles,
is that guideline applies to manhole as well? What you thing about this?
SnTMan, I believe the OP is referring using a weld neck rather than slip-on when operating at elevated temperatures. Even if not mandated, a lot of specifications will limit the maximum temperature for slip-on flanges. Thermal stress caused by temperature differentials can lead to cracking at SO fillet welds when operating at elevated temperatures. I would think it would be worse for process nozzles since the thermal transient would be more severe where the flow rate is higher at the flange vs a manhole flange, which is why I was suggesting the 'thermal' shock would be less severe. Under steady state conditions it makes no difference.
Not very helpful without the figures but the rough translation appears to be orifice flanges, is this the case? You wouldn't have an orifice flange on a manhole so the P-T limit would not be applicable to this case. Might be best to clarify your question.
PD 5500 -2015 Fillet welded pipework flanges shall not be used for design temperatures above 370 °C
EN 13445 Flange construction . Fillet welds shall not be used for design temperatures above 370 °C.