Apr 7, 2018 #1 jor1492 Mechanical Joined Aug 3, 2015 Messages 106 Location PA Hello All, In your experience do you recommend a system of cathodic protection (impressed or galvanized) for a Carbon steel Pipeline of Diesel running above the ground (not buried)? For information the life of the plant will be 50 years.
Hello All, In your experience do you recommend a system of cathodic protection (impressed or galvanized) for a Carbon steel Pipeline of Diesel running above the ground (not buried)? For information the life of the plant will be 50 years.
Apr 7, 2018 1 #2 mk3223 Mechanical Joined Feb 4, 2006 Messages 1,488 Location US The cathodic protection is for the underground pipeline. Suggest to use an external painting to protect the aboveground pipeline. Upvote 0 Downvote
The cathodic protection is for the underground pipeline. Suggest to use an external painting to protect the aboveground pipeline.
Apr 7, 2018 1 #3 LittleInch Petroleum Joined Mar 27, 2013 Messages 23,008 Location GB Cathodic protection of any kind DOES NOT WORK on above ground pipelines. Look very carefully at the points where the pipe is supported. They are usually the points where corrosion occurs. Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote
Cathodic protection of any kind DOES NOT WORK on above ground pipelines. Look very carefully at the points where the pipe is supported. They are usually the points where corrosion occurs. Remember - More details = better answers Also: If you get a response it's polite to respond to it.
Apr 9, 2018 Thread starter #4 jor1492 Mechanical Joined Aug 3, 2015 Messages 106 Location PA thanks guys Upvote 0 Downvote