Based on ASME SecI PW11 it is needed for one of our HP Drums to be full RT , but our licensor have told us to do 100% RT and 100% UT on all circumferrential and longitudinal butt welds of the drum. (The drum tickness is 90mm and the pressure is about 150bar). what kind of defect can we find by UT which we can not find by radiography?