Is there a method of sending a probe down a pipeline (underground) to measure wall thickness?
 
Replies continue below

Recommended for you

Search:
- "smart pigs"
- "pipeline pigging"
- and variation thereof.

"Smart Pigs" used quite often in the oil & gas industries to inspect underground pipelines.


Vita sine litteris mors est.
 