Sep 8, 2005 #1 ddiliberto New member Joined Sep 2, 2005 Messages 7 Location DE Do anybody knows an NDI inspection which permit to discover corrosion in the bore of an hole in which is installed a bushing?
Do anybody knows an NDI inspection which permit to discover corrosion in the bore of an hole in which is installed a bushing?
Sep 8, 2005 #2 berkshire New member Joined Jun 8, 2005 Messages 4,429 Location US Have you tried ultrasound at a tangent? B.E. Upvote 0 Downvote
Sep 9, 2005 Thread starter #3 ddiliberto New member Joined Sep 2, 2005 Messages 7 Location DE Thank you Berkshire, I will try your solution too. In the meantime I found the following company, which is proposing a dedicated technology http://www.imtt-usa.com/products_othercrackdetectionprobes_crack_bsh.html Regards Upvote 0 Downvote
Thank you Berkshire, I will try your solution too. In the meantime I found the following company, which is proposing a dedicated technology http://www.imtt-usa.com/products_othercrackdetectionprobes_crack_bsh.html Regards