Hi,
What does mean NDE Procedure Demonstration to an AI?
I particulary want to know that, what will an AI ask during UT Procedure Demonstration?
Pls. guide me in detail.
Thanks in advance
BPVN
 
Replies continue below

Recommended for you

BPVN;
In simple terms, it means that the ultrasonic test examination procedure(s) for your NDT program is reviewed and your Level II or Level III will use this procedure on a reference block for the AI.
 
Hi Metengr,
Thanks for quick reply. But could you pls. explain some more that, how to Demonstrate UT Procedure to AI and during Demonstration, Generally what will AI ask? i.e Questions?
Pls. guide me.
Thanks
 
Typically, the AI would want to determine if you know how to use your own, written and qualified UT procedure to find manufactured flaws in a reference block.
 