Most companies require NDE to be performed after PWHT for P1 materials, however, I cannot find this as being a requirement anywhere in B31.3. I find it interesting that B31.3 states that leak testing should take place after PWHT (implying to me that soundness should be checked for for after PWHT),however, no where does it state that NDE on P1 material should be done after PWHT, which is also a check for soundness. Any thoughts?