anyone have more than the E rivets in MMPDS-01 ? sure i can scale for AD material, but if anyone's got anything it be appreciated.

another day in paradise, or is paradise one day closer ?
 
You shoulda taken 'em when I offered 'em the first time. Nah, just kidding, see file attached below. But don't blame me for the scan quality.

Deriving a value for "AD" material from "E" data has been shown to be non-conservative.
The enclosed are test values.

If anyone can find a copy of the original report, Grumman GE-148, I'd be very grateful, and owe them at least a round at the pub.
(Crackman, are you listening??? [wink])

STF
 
 http://files.engineering.com/getfile.aspx?folder=67f34366-abd3-4c17-b86b-144ed7220e60&file=Grumman_NAS1097AD_Rivet_Data.pdf
thx Ed ... that was for dimpled skins (yeah, i know, i didn't say). interesting how much more effective dimpled skin are. I've attached my read of sparweb's Grumman data.

another day in paradise, or is paradise one day closer ?
 
 http://files.engineering.com/getfile.aspx?folder=e6f49460-f645-4409-a625-ef773c2bcd0a&file=NAS1097.xlsx