At what concentration of H2S would you use a NACE trim PRV set 1440 psi

JAC
 
Replies continue below

Recommended for you

If any of the pressure containing parts, or wetted parts necessary for the correct functioning of the valve, are other than carbon or low alloy steel, then it would be any concentration above zero ppm

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
SJones,

I am involve in a produced water project where I need to recommend either Carbon steel or Carbon Steel (NACE) for the service.

I need to know the threshold required to determine whether a NACE material is required or not.