Hi,

I woul like to qualify a martensitic stainless steel which isn't listed in MR0175-part 3. I have a question to users of the NACE MR0175 norm.
Because that kind of material is considered as corrosion-resistant alloy (CRA), I am not sure of the right thing to do.

First, CRA are described on MR0175-3, and the only description to qualify these materials is given on annex B (by using Annex E and TM0177). That annex explains how to qualify it by laboratory service.

Moreover, paragraph 8.2 from MR0175-1 gives requirements for a qualification based upon field experience. Contrary to MR0175 - part 3 which is specific to CRA, part 1 deals with materials in general for H2S environment.

Do I really have to use MR0175 part 3 ? Or is it possible to follow simply MR0175 part 1 requirements ?
 
If you cannot use the Annex A tables of Part 3, you have the two options available to you that are stated in Part 1, and reiterated in subclause 6.1, paragraph 5 of Part 3: documented service experience, or laboratory testing.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top