We are a valve manufacture that builds everything to order-not to stock.
We often get request for a specific material to MRO 0175 or MRO 0103 (and no mention of the year of the spec.)
Is there a summary available that states the difference between the two standards for:
316/316L and CF8M/CF3M
Hastelloy B and C grades
I see the max hardness and the chemistry requirment, but I am concerned I am missing something
We often get request for a specific material to MRO 0175 or MRO 0103 (and no mention of the year of the spec.)
Is there a summary available that states the difference between the two standards for:
316/316L and CF8M/CF3M
Hastelloy B and C grades
I see the max hardness and the chemistry requirment, but I am concerned I am missing something