In Par. 3.2 of NACE MR 0175, only a restricted number of heat treatment conditions are allowed: hot rolled, annealed, normalized, normalized and tempered, normalized + austenized + quenched + tempered, austenized + quenched + tempered.
Some heat treatment conditions like thermomechanical rolling or normalizing rolling are not included.
In appendix D, table D1, pipes up to API-5L X65 are considered as acceptable material. Or practically all X65 material is thermomechanical rolled.
Does someone has more information about the choice of NACE?
 