Mar 15, 2011 #1 alseng Petroleum Joined Feb 1, 2011 Messages 7 Location TN thread338-193495 NACE MR0176 is used for listed metallic materials for subsurface sucker rod pumps for hydrogen sulfide environments. wich goes in parallel with the API (American Petroleum Institute) specification 11AX.
thread338-193495 NACE MR0176 is used for listed metallic materials for subsurface sucker rod pumps for hydrogen sulfide environments. wich goes in parallel with the API (American Petroleum Institute) specification 11AX.