I have searched this topic and I can't find the information.

Question:
Is there an upper concentration limit for the NACE MR0175?

Example:
I can see that for carbon steels Rc22 is the max hardness to operate in the SCC zone as depicted by MR0175. But the charts in MR0175 show a limited pressure range and concentration range.

So - would I still be good with this standard if I know that I would be operating at 50% H2S at 10,000 psi? It would definately be in the SCC zone, but would the concentration and the pressure affect the Rc22 rule?

Please advise.

jackboot
 
Replies continue below

Recommended for you

I have been involved in much SSC testing of steels for oil/gas production. The upper limit hardness is a function of pH and H2S concentration. There isn't much published on this. Since steel with 22 HRC hardness can withstand 100% H2S (e.g. testing according to NACE TM0177), you should be okay with the 50% concentration.

Regards,

Cory