Can somebody please explain to me the difference between a 3mm NACE CA and a 3mm Non-NACE CA? Thank you.
 
Replies continue below

Recommended for you

The former is a 3mm corrosion allowance in material rated for sour service. The latter is a 3 mm corrosion allowance in material NOT rated for sour service. Technically, as they are both corrosion allowances, there is no difference between them.