hi
Ive been trying to find a standard for installing NACA slug rivets, and was wondering if anyone's had the pleasure of working with slug rivets ... what standard did they refer to?
 
Replies continue below

Recommended for you

median..

Acft manufacturer specs are probably the best bet. Try Boeing BAC5047 & BAC5047-1.

Otherwise... You are stuck with NASM47196.

Regards, Wil Taylor
 
Media.. forgot to add BAC5047-2.

Regards, Wil Taylor
 
In case you still haven't a copy of NAS47196, you could look up MIL-R-47196 on the DOD's ASSIST website. It's an older version, but it's free.


Steven Fahey, CET
 
thanks sparweb, it was a hastle trying to locate the standards wktylor mentioned.
 