Hi there,

I'm researching for info on Mystik 7455 tape, a high temp. Aluminum/Glass cloth tape and getting very few leads at the moment. I was wondering if there might be any definite sites or repositories that may carry technical info, specs, application and descriptions on this item. Assistance in this is much appreciated as I'm not having much luck at the moment.

Thanks,
Silverspeed

 
Why not contact the Manufacturer?

Duck Tape has a history of usage on their website for duct tape.

TTFN
 
This is a direct solution when the name of the product's manufacturer is available for reference, but not in this case. FYI, It wasn't provided by the distributor (despite a request) until after it's use was deemed redundant. Thanks for the reply.

Ss
 
Silverspeed,

I checked with one of my suppliers, and he couldn't even find a cross-reference to that tape.

Are you looking to match a current tape with the Mystik tape? At the very least, I can hook you up with some samples of some foil/glass tapes (which I can get specs for), though I realize from your post you are trying to find specs for the 7455 tape.

Let me know if I can be of any help.

Dave
 
silverspeed,

I have some information on the strength and use of this tape. It meets MIL-T-83284. I am looking for the density of this particular tape. I see it has been awhile since this was first posted. Have you found any more information?
 