Can concrete increase entrained air content from the on site air test to hardened air content?
Equipment calibrations, cylinder weights and finishing all indicate a no air mix for this interior slab at 2-3%.
18 months later, they are witnessing delamination. Cores were taken and tested for hardened air content at 7%.
We tried a trial batch, checking the air content before and after adding water at the jobsite. No change in air.
What else can we investigate with this?
Thanks in advance
Equipment calibrations, cylinder weights and finishing all indicate a no air mix for this interior slab at 2-3%.
18 months later, they are witnessing delamination. Cores were taken and tested for hardened air content at 7%.
We tried a trial batch, checking the air content before and after adding water at the jobsite. No change in air.
What else can we investigate with this?
Thanks in advance